Measurement |
Condition |
Value |
Viscosity |
@ 26 °C (78.8 °F) |
450-520 cps |
Color |
White |
|
Density |
@ 25 °C (77 °F) |
1.12 g/cm³ |
Ec(critical exposure) |
Dp(slop of cure-depth vs.ln(E) curve) |
8.5-9.3 mJ/cm2 |
0.125-0.14 |
ASTM Method |
Property Description |
Value |
ASTM D 638 |
Tensile Modulus |
2540-2720 MPa |
ASTM D 638 |
Tensile Strength at Break |
45-53 MPa |
ASTM D 638 |
Elongation at Break |
7-10% |
ASTM D 648 @66PSI |
Heat Deflection Tempertature |
50-55℃ |
ASTM D 790 |
Flexural Strength |
60-75Mpa |
ASTM D 790 |
Flexural Modulus |
2080-2350Mpa |
ASTM D 256 |
Izod Impact (Notched) |
20-30 J/m |
ASTM D 2240 |
Hardness Shore D |
81-85 |