Measurement |
Condition |
Value |
Viscosity |
@ 27 °C (80.6 °F) |
300-380 cps |
Color |
White |
|
Density |
@ 25 °C (77 °F) |
1.121 g/cm³ |
Ec(critical exposure) |
Dp(slop of cure-depth vs.ln(E) curve) |
9.0-9.9 mJ/cm2 |
0.125-0.135 |
ASTM Method |
Property Description |
Value |
ASTM D 638 |
Tensile Modulus |
2270-2380 MPa |
ASTM D 638 |
Tensile Strength at Break |
43-48 MPa |
ASTM D 638 |
Elongation at Break |
8 -11% |
ASTM D 648 @66PSI |
Heat Deflection Tempertature |
56-60℃ |
ASTM D 790 |
Flexural Strength |
62-70 Mpa |
ASTM D 790 |
Flexural Modulus |
2312-2401 Mpa |
ASTM D 256 |
Izod Impact (Notched) |
18-30 J/m |
ASTM D 2240 |
Hardness Shore D |
81-85 |